2016年10月27日星期四

ASTM A709 Grade HPS70W steel




For quenching and tempering treatment, the steel should be heated to not less than 1650oF [900oC], water quenching or oil quenching and tempering temperature is not lower than 1100oF [590oC].
ASTM A709 Grade HPS70W structural steel in hot selling,we have many ASTM A709 Grade HPS70W steel in stock,if you need ASTM A709 Grade HPS70W structural steel,please feel free to contact katalor!